Grain Alkane Mapping align ContactMode Adhesion cannabis Water NUS SmalScan LaAlO3 Co/Cr/Pt BTO blended polymers OpticalWaveguides ElectroDeposition LiNbO3 Mosfet Hafnium_dioxide TCS Barium_titanate layers IMT_Bucharest Hair INSP Implant Aggregated_molecules StrontiumTitanate PhthalocyaninePraseodymium Collagen molecules ScanningSpreadingResistanceMicroscopy exfoliate Workfunction AIN
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2 (1/2)
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 30μm×30μm
- Scan Rate: 0.1Hz
- Pixel: 512×1024