PolyimideFilm PMNPT TappingMode Cobalt-dopedIronOxide rubber Temperature DLaTGS LightEmission HafniumDioxide Materials Lateral Gong CuSubstrate C60H122 Modulus Multiferroic_materials ForceVolume Insulator FailureAnalysis ImideMonomer Polyvinylidene Ferrite NUS_Physics Trench StrontiumTitanate Ni81Fe19 CalciumHydroxide LogAmplifier temp Al2O3 Tin disulfide SiWafer LifeScience PFM Techcomp
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer patterns on Si (2/2)
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.2Hz
- Pixel: 512×256