Temperature Sadowski Pores Bio CeramicCapacitor Sic suspended_graphene Metal Molybdenum_disulfide MESA structure PhthalocyaninePraseodymium CP-AFM GaAs Mapping 2d_materials oxide_layer rubber Microchannel Current LiftMode MLCC plastics alkanes cooling PetruPoni ElectroDeposition self-assembled_monolayer Corrosion P3HT Chrome Pipette Dopped neodymium_magnets China LMF
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
AEAPDES Self-Assembly monolayer
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 0.25μm×0.25μm
- Scan Rate: 1.5Hz
- Pixel: 256×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 0.25μm×0.25μm
- Scan Rate: 1.5Hz
- Pixel: 256×256