Optic Vac Worcester_Polytechnic_Institute Conductivity Co/Cr/Pt BaTiO3 suspended_graphene DeoxyribonucleicAcid VerticalPFM LateralForceMicroscopy Optoelectronic domain_switching Photovoltaics Chromium F14H20 blended polymers LiftMode MagneticPhase self-assembled_monolayer Optoelectonics Steps AlkaneFilm NUS_Physics Scanning_Thermal_Microscopy NUS_NNI_Nanocore MolybdenumDisulfide Tungsten_disulfide SRAM Polypropylene Nickel #EC ForceVolume HexacontaneFilm norganic YttriaStabilizedZirconia
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Hard disk media
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 0.250μm×0.250μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 0.250μm×0.250μm
- Scan Rate: 0.5Hz
- Pixel: 512×512