Writing Switching light_emission molecular_beam Global_Comm Current SoftSample PS_PVAC Mechinical ScanningKelvinProbeMicroscopy Lateral_Force_Microscopy LiftMode Singapore domain_switching Tape NTU UnivOfMaryland ContactModeDot mechanical property NUS Nanostructure ThermalProperties BariumTitanate Fluoride WS2 Ananth TransitionMetal Anneal LeakageCurrent P3HT Spain Vortex Pinpoint PFM TiO2 AmplitudeModulation
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polyurethane
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact, TCS
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 512×256