MultiLayerCeramicCapacitor bias_mode FrictionalForce Gong SmalScan AmplitudeModulation LithiumNiobate FFM suspended_graphene Hydroxyapatite Polarization Forevision SPMLabs Tin disulfide pinpoint mode Aluminum KevlarFiber UnivCollegeLondon norganic Sidewall PolycrystallineFerroelectricBCZT SingleLayer Piezoelectric AAO Edwin biocompatible StrontiumTitanate Korea ThermalDetectors CP-AFM BlockCopolymer cannabis Nanopattern Corrosion BiVO4
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/PVAc Film
Film of Polystyrene/poly(vinyl acetate) blend on Si
Scanning Conditions
- System: NX20
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au C (k=0.6N/m, f=65kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.3Hz
- Pixel Size: 1024 × 256
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au C (k=0.6N/m, f=65kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.3Hz
- Pixel Size: 1024 × 256