Growth Terrace FM_SKPM Deposition PUR CaMnO3 Array Insulator Thermal Ni-FeAlloy Worcester_Polytechnic_Institute IcelandSpar Nanostructure Step norganic DLaTGS Ram PtfeFilter silicon_oxide NeodymiumMagnets Fe_film temp Styrene Force-distance Patterns PVAP3HT #Materials INSP Organic TyphimuriumBiofilm Pore Varistor ScanningSpreadingResistanceMicroscopy NCM\ AmplitudeModulation
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Margarines
Phase change of Margarine surface by temperature control
Scanning Conditions
- System: NX10
- Scan Mode: Tapping, TCS1
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1.2Hz
- Pixel Size: 256 × 256