SingleLayer HexagonalBN SThM cannabinoid Sadowski SICM FrictionalForce CuSubstrate I-VSpectroscopy MolecularSelfAssembly Roughness CuFoil Al2O3 Laser Zagreb Pores SetpointMode TemperatureControllerStage Hexatriacontane self_assembly CeramicCapacitor ScanningKelvinProbeMicroscopy CntFilm WWafer temp DOE PMNPT Inorganic_Compound SurfaceOxidation Polyvinylidene Terrace VerticalPFM Wafer BreastCancerCell UnivOfMaryland
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Semi-fluorinated alkanes
Scanning Conditions
- System : NX10
- Scan Mode: Sideband KPFM
- Scan Rate : 0.4 Hz
- Scan Size : 500nm×500nm
- Pixel Size : 256×256
- Cantilever : HQ: NSC14/CR-AU (k=5N/m, f=160kHz)