AlkaneFilm MagneticForce Annealing Perovskite MeltingPoint Beads Workfunction PS_LDPE SetpointMode nanobar ReflexLens Liquid HACrystal cannabis INSP SRAM Hafnium_dioxide ring shape Topography cannabinoid organic_polymer Aluminium_Oxide Gallium_Arsenide Pvdf Hydroxyapatite FastScan ThermalDetectors MetalCompound IndiumTinOxide blended polymers STO Hafnia Polyvinylidene BloodCell BiVO4
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Galfenol (Alloy of iron and gallium)
Scanning Conditions
- System: XE15
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=70kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- MFM Lift height: 50nm