Tin disulfide Vacuum molecular_self_assembly LiftMode Sadowski Corrosion BismuthFerrite vertical_PFM food LightEmiting Protein pulsed_laser_deposition Pipette Holes Mechinical MfmAmplitude Nanopattern PS_PVAC MechanicalProperty UnivOfMaryland non_contact SiWafer ElectrostaticForceMicroscopy semifluorinated alkane ScanningKelvinProbeMicroscopy GlassTemperature MetalCompound SrTiO3 University_of_Regensburg hydrocarbon LFM Force-distance Polydimethylsiloxane HexagonalBN PhaseImaging
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic device
Scanning Conditions
- System : NX20
- Lift Height : 50nm
- Scan Mode: MFM
- Scan Rate : 0.3Hz
- Scan Size : 20μm×20μm
- Pixel Size : 512×256
- Cantilever : PPP-MFMR (k=2.8N/m, f=75kHz)