Memory Beads Trench Magnetic Force Microscopy Styrene Piezoresponse multi_layer FFM DIWafer PS_LDPE fe_nd_b Sio2 AmplitudeModulation MetalCompound Current BiasMode DentalProsthesis Writing IIT-chennai Tape Carbon Friction Optical DeoxyribonucleicAcid Layer Hair INSP LiNbO3 Electronics Oxidation HardDiskMedia Dimethicone HanyangUniv TempControl Polarization
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cutting Graphene
Scanning Conditions
- System : FX40
- Scan Mode: Contact after lithography
- Scan Rate : 0.7 Hz
- Scan Size : 30μm×30μm
- Pixel Size : 256×256
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)
- Lithography condition : Force 500 nN, writing speed 0.1μm/s, AC bias 10 V @ 40kHz