Vinylpyridine Lanthanum_aluminate PolyvinylideneFluoride Global_Comm IMT_Bucharest semifluorinated_alkane Piezo temperature_control KPFM Spincast Platinum mechanical_property self-assembled_monolayer SingleCrystal MembraneFilter LogAmplifier Led Polypropylene Etch PANI Galfenol Monisha Permalloy SurfaceOxidation hydrocarbon LFM Butterfly ShenYang Collagen Flake Optoelectonics Gallium_Arsenide rubber Lattice Display
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Domain switching on PZT
Scanning Conditions
- System: NX10
- Scan Mode: Lithography, PFM
- Cantilever: ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Litho. mode: Tip bias mode
- Litho. Tip bias: Black +10V, White -10V