Chungnam_National_University Hole BismuthVanadate epitaxy temperature controller AFM Foil Resistance ferromagnetic FM-KPFM Ceramic WWafer Pvdf PhaseTransition WPlug Electronics Bmp UTEM MagneticForceMicroscopy TiO2 Nanotechnology Inorganic_Compound ScanningTunnelingMicroscopy self_healing thermal_conductivity Topography NTU Kevlar MagneticArray LiquidImaging Litho UnivOfMaryland SrO AM_KPFM EPFL Glass
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG Moire
Scanning Conditions
- System: NX10
- Scan Mode: STM
- Cantilever: Pt wire
- Scan Size: 2.5μm×2.5μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 0.3Hz, 1Hz, 2Hz
- Pixel: 512×256, 512×256, 256×128