Inorganic MfmPhase LiquidCell epitaxy MagneticForce layers MultiferroicMaterials molecular_self_assembly Titanate Magnetostrictive SurfaceChange CrossSection HighAspect mono_layer nanobar ConductiveAFM cannabis LiquidImaging Insulator Change C_AFM Nickel atomic_steps bias_mode BismuthFerrite ScanningTunnelingMicroscopy Tin disulfide EFM LifeScience IndiumTinOxide InsulatorFilm pulsed_laser_deposition SoftSample PtfeFilter TungstenDeposition
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
NiFe
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.2μm×1.2μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- Lift height: 20nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.2μm×1.2μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- Lift height: 20nm