plastic Granada FrictionForce Zagreb sputter AnodizedAluminumOxide BTO BloodCell FFM Epoxy Aluminium_Oxide Defect silicon_carbide Ucl Chemical_Vapor_Deposition Change BariumTitanate LeakageCurrent Perovskite atomic_steps Regensburg ring shape TappingMode Collagen food Composite ScanningSpreadingResistanceMicroscopy oxide_layer aluminum_nitride SelfAssembly LateralForceMicroscopy OxideLayer FM_SKPM NeodymiumMagnets ForceVolumeImage
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Alkane Film (C60H122)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512