HighResolution Indium_tin_oxide Chloroform PFM Solution C_AFM Bmp Inorganic_Compound Perovskite cannabinoid PhthalocyaninePraseodymium Display Forevision ULCA NUS StrontiuTitanate ElectroDeposition Gong PDMS Oxidation Spincast PatternedSapphireSubstrat Mobile DIWafer Titanate Sphere Nanopattern Electrical&Electronics Film SICM C36H74 GlassTemp HexagonalBoronNitride CeramicCapacitor Pinpoint PFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
AlSbAs
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 1Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 1Hz
- Pixel: 512×512