MfmAmplitude Memory exfoliate Varistor Self-assembledMonolayer Reduction Pzt Nickel blended polymers Hexacontane PatternedSapphireSubstrat Techcomp LiIonBattery BismuthVanadate TipBiasMode nanobar AAO Sapphire Mapping TungstenDeposition Tapping Oxide LeakageCurrent FM-KPFM high_resolution neodymium_magnets Bacteria HardDisk #Materials AM_KPFM amplitude_modulation BaTiO3 FrictionalForceMicroscopy Insulator Polytetrafluoroethylene
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer blend with nanofiber
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 512×512