ForceVolumeImage CntFilm LiBattery BFO Galfenol Oxide Calcite PvdfBead oxide_layer Treatment cross section Adhesive NUSNNI dielectric_trench Cobalt Patterns align CrossSection Plug SingleCrystal cannabis neodymium_magnets CompactDisk AAO Lateral_Force_Microscopy Temasek_Lab Celebration Conduct GranadaUniv CuFoil Piezo InLiquid STO GalliumPhosphide PUR
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/PVAc Film
Film of Polystyrene/poly(vinyl acetate) blend on Si
Scanning Conditions
- System: NX20
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au C (k=0.6N/m, f=65kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.3Hz
- Pixel Size: 1024 × 256
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au C (k=0.6N/m, f=65kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.3Hz
- Pixel Size: 1024 × 256