Biofilm StainlessSteel HOPG ElectrostaticForceMicroscopy TriGlycineSulphate thermal_conductivity CrAu aluminum_nitride Croatia semifluorinated alkane Magnets Optic TyphimuriumBiofilm fifber ScratchMode Domain #EC semifluorinated_alkanes HighAcpectRatio Optical MetalCompound GalliumPhosphide CBD Solar ScanningTunnelingMicroscopy SurfaceOxidation H-BN InLiquid RedBloodCell IISCBangalore Varistor C_AFM silicon_carbide AM_SKPM Floppy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Crosslinked starch & pectin fibers
Scanning Conditions
- System : NX-Wafer
- Scan Mode: Tapping
- Scan Rate : 0.31 Hz
- Scan Size : 15μm×15μm
- Pixel Size : 256×256
- Cantilever : ContSCR (k=0.2N/m, f=25kHz)