Phase sputter Hole Inorganic_Compound HiVacuum Nanotechnology FM_SKPM CP-AFM MfmPhase I-VSpectroscopy Mosfet ChemicalCompound TempControl Deposition Spain MolecularSelfAssembly Chemical Vapor Deposition ScanningTunnelingMicroscopy ForceDistanceSpectroscopy DeflectionOptics TPU LightEmiting HexagonalBoronNitride mfm_amplitude Yeditepe ScratchMode oxide_layer PolymerBlend PVAP3HT DomainSwitching pulsed_laser_deposition alkanes Fujian nanobar Litho
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
TSV Cu pad oxidation
Scanning Conditions
- System : NX-Wafer
- Scan Mode: Non-contact
- Scan Rate : All 1 Hz
- Scan Size : 40μm×40μm
- Pixel Size : All 512×512
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)