Croatia Current SRAM Sidewall CopperFoil CalciumHydroxide Ucl AAO SPMLabs Pvdf NtuEee FastScan Floppy layers Display self_healing Barium_titanate block_copolymer India rubber Au111 Optoelectonics Reading FrequencyModulation StainlessSteel Hafnium_dioxide DIWafer ThermalConductivity InLiquid Led Polydimethylsiloxane Beads PinpointNanomechanicalMode Fiber Wildtype
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Gold(111) coated mica substrate
Scanning Conditions
- System: XE7
- Scan Mode: Contact
- Cantilever: PPP-ContScR (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 256×256
- EC electrode: Ag/AgCl2(Reference electrode), Pt(Counter electrode), CuSO4(0.1mM) + H2SO4(0.01mM)(Electrolyte)
- EC bias voltage: -0.3V