Styrene CeramicCapacitor Anneal DLaTGS biocompatible Moire CompactDisk CntFilm DiffractiveOpticalElements GlassTemp Granada light_emission hetero_structure Alkane Hexacontane Oxide Vanadate NeodymiumMagnets GalliumPhosphide Nanopattern Biology HydroGel MBE StainlessSteel Flake SrO PtfeFilter PpLdpe China GlassTemperature Yttria_stabilized_Zirconia ShenYang Piezoelectric Water Ito
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic patterned array
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.7μm×1.7μm
- Scan Rate:0.5Hz
- Pixel:256×128