Yeditepe_University Cell PVA Ferroelectric BaTiO3 SiliconOxide Co/Cr/Pt LMF Photovoltaics VerticalPFM Zhi single_layer Styrene BTO Stiffness Molybdenum_disulfide Bmp Resistance molecular_self_assembly Oxidation BoronNitride PhaseImaging PyroelectricDetector UnivCollegeLondon Growth LiBattery Reduction Ceramics SurfaceChange mono_layer BFO SSRM Magnets align Neodymium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Suspended single-layer Graphene
Single-layer Graphene is suspended on microchannels fabricated on Si/SiO2 substrate.
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: Access-NC (k=113N/m, f=330kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.4Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: Access-NC (k=113N/m, f=330kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.4Hz