AtomicLayer Water Edwin InorganicCompound electrospinning Led SiliconeOxide FrictionalForceMicroscopy Reduction Litho Hexacontane PiezoelectricForceMicroscopy Liquid VinylAlcohol Lateral hard_disk_media FM_SKPM Permalloy Zhi PvdfFilm Fiber conductive hydrocarbon Hafnium_dioxide Terrace Pore Resistance blended polymers Writing Crystal norganic Growth Alkane MolecularSelfAssembly Organic
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Spincast layer of PS/LDPE blend on Si.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256