Hafnia AmplitudeModulation Lift Semiconductor ferromagnetic AEAPDES TipBiasMode Worcester_Polytechnic_Institute Holes amplitude_modulation TiO2 NUS_NNI_Nanocore Fendb Graphite CopperFoil CntFilm food Flake Copolymer ReflexLens Trench Piezoelectric BismuthVanadate TransitionMetal CeramicCapacitor KevlarFiber PinPointMode Ni-FeAlloy Potential Ni81Fe19 PinpointNanomechanicalMode Wonseok Reading Bacterium graphene_hybrid
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Triple-cation perovskite
Scanning Conditions
- System : NX10
- Sample bias: 0 V, 0.5 V
- Scan Mode: C-AFM with PCM toolkit
- Scan Rate : 0.25 Hz
- Scan Size : 5μm×5μm
- Pixel Size : 512×512
- Cantilever : ANSCM-PC (k=0.2N/m, f=12kHz)