Growth SKKU PolyimideFilm plastics Tape BismuthFerrite PinPointMode Spain domain_switching P3HT FM_KPFM Neodymium Yeditepe TCS molecular_self_assembly Polystyrene BreastCancerCell Dental Hexatriacontane amplitude_modulation Molybdenum Phosphide PhthalocyaninePraseodymium mechanical property LowDensityPolyethylene Epoxy Kevlar STM silicon_oxide Vac FrequencyModulation Cobalt DiffractiveOpticalElements SurfaceOxidation Lattice
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PZT thin film
Scanning Conditions
- System: NX10
- Scan Mode: PFM (DC-EFM)
- Cantilever: ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 512×512