Alkane Annealed dielectric_trench I-VSpectroscopy layers Oxidation WS2 ScanningThermalMicroscopy AM_SKPM MeltingPoint lithography cannabis Tungsten_disulfide Sadowski Cross-section LDPE Boron ConductingPolymer Wang BoronNitride ForceVolumeImage Monisha Hydroxyapatite VinylAlcohol molecules Heating Christmas self_assembly TungstenThinFilmDeposition MagneticForce HardDisk SPMLabs Multiferroic_materials Gallium_Arsenide NiFe
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic patterned array
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.7μm×1.7μm
- Scan Rate:0.5Hz
- Pixel:256×128
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 1.7μm×1.7μm
- Scan Rate:0.5Hz