MagneticArray Lift AEAPDES BFO NeodymiumMagnets Annealed HanyangUniv UTEM WPlug Lattice Moire IMT_Bucharest CVD ContactMode FastScan BiFeO3 Metal-organicComplex Adhesion Chemical Vapor Deposition HydroGel CancerCell fluoroaalkane ring shape TappingMode PvdfFilm Display ferromagnetic ChemicalCompound Sic GlassTemperature STO Optical YszSubstrate Dr.JurekSadowski Ca10(PO4)6(OH)2
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Graphene on SiO2
Scanning Conditions
- System: NX20
- Scan Mode: PinPoint mechanical mode
- Cantilever: NSC36C
- Approach/Retract speed : 2ms/2ms
- Scan Size: 10μm×10μm, 5μm×5μm
- Pixel: 256 × 256
- Scan Mode: PinPoint mechanical mode
- Cantilever: NSC36C
- Approach/Retract speed : 2ms/2ms
- Scan Size: 10μm×10μm, 5μm×5μm
- Pixel: 256 × 256