BariumTitanate Barium_titanate Sperm membrane hard_disk_media Wang Optic HighAspect F14H20 epitaxy Typhimurium Pinpoint sputter ScanningIon-ConductanceMicroscopy semifluorinated alkane cooling HOPG FailureAnalysis Pyroelectric H-BN NTU Led Imprint Ferroelectric Christmas Polyaniline Optoelectonics KelvinProbeForceMicroscopy IMT_Bucharest TempControl AnodizedAluminumOxide VortexCore Topography temperature_control Moire
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
AlN/GaN/AlN Hetero Structure
AlN/GaN/AlN hetero structure grown on SiC substrate by Molecular Beam Epitaxy (MBE) system.
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 512