Polymer ForceVolumeMapping Sio2 Hole Layer Pyroelectric AM-KPFM C_AFM 3-hexylthiophene fluorocarbon Laser C36H74 EPFL Growth BloodCell Polyvinylidene Yttria_stabilized_Zirconia IcelandSpar Varistor Dimethicone align Floppy HighAspect ChemicalCompound pulsed_laser_deposition NUS_NNI_Nanocore Boron Worcester_Polytechnic_Institute CalciumHydroxide StrontiuTitanate AdhesionForce Gong Thermal HumanHair Oxide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2 into Indium Tin Oxide Film
ITO film on 1% HfO2-doped Yttria-stabilized Zirconia (001) orientation grown by pulsed laser deposition. Surface segregation of HfO2 into ITO film.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256