MeltingPoint Ferroelectric Ferrite pinpoint mode Mechanical&nanotechnology TransitionMetal HanyangUniv Chrome BreastCancerCell solar_cell Layer SThM Hexatriacontane MBE MultiferroicMaterials Switching Varistor exfoliate atomic_steps TempControl KPFM SurfaceChange NUS_Physics Hole margarine temperature controller AFM Co/Cr/Pt Kevlar vertical_PFM Protein CastIron Liquid suspended_graphene PolyvinylAcetate IIT-chennai
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ferromagnetic Nanobars Array
Ferromagnetic nanobars arranged on a Penrose P2 tiling. The Permalloy (Ni81Fe19) nanobars are 810 nm and 500 nm long. The width and thickness of a nanobar amount to about 120 nm and 25 nm, respectively.
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 7μm×7μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Lift height: 85nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 7μm×7μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Lift height: 85nm