InLiquid Fendb MonoLayer Polystyrene PvdfBead PinpointNanomechanicalMode GalliumPhosphide Mfm PolyimideFilm AnodizedAluminumOxide PetruPoni_Institute Barium_titanate C36H74 GaAs SRAM AdhesionForce Liquid DeflectionOptics mechanical property Solar SThM FAFailureAnlaysis Array Indium_tin_oxide Hydroxyapatite ContactModeDot DNA INSP Piezoresponse HardDisk MagneticPhase margarine self-assembled_monolayer Magnetic TungstenDeposition
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
C36H74
Layer of C36H74 alkane on HOPG.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256