LaAlO3 Tungsten HydroGel Ca10(PO4)6(OH)2 SSRM heterojunctions nanomechanical ForceVolumeImage semifluorinated alkane PVAC SelfAssembly CalciumHydroxyapatite Wang Insulator MechanicalProperties Growing MagneticPhase VinylAlcohol 3-hexylthiophene DNAProtein P3HT #Materials ThermalDetectors EvatecAG Subhajjit Aluminium_Oxide 2-vinylpyridine Potential Writing PhaseImaging Mobile OpticalModulator Monisha PVAP3HT light_emission
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2 (2/2)
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au(k=1N/m, f=90kHz)
- Scan Size: 30μm×30μm,10μm×10μm
- Scan Rate: 0.1Hz
- Pixel: 512×1024