Hafnium_dioxide CHRYSALIS_INC Oxidation Silver ThermalProperties cooling ThermalDetectors CaMnO3 Mosfet Nickel TransitionMetal Granada piezoelectric force microscopy Hair Force-distance organic_polymer SingleCrystal PS_LDPE PVAC India fluoroalkane CrAu EFM cannabis Growing NCM\ Heating Led Dr.JurekSadowski block_copolymer HiVacuum Pipette Vinylpyridine alkanes TempControl
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Graphene
Scanning Conditions
- System: XE7
- Scan Mode: Conductive AFM
- Cantilever: NSC36C Cr-Au (k=0.6N/m, f=65kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 256×256