India TransitionMetal PECurve 3-hexylthiophene AM_KPFM Battery WS2 fluorocarbon Melt PhthalocyaninePraseodymium DomainSwitching Sic Sadowski PtfeFilter PANI GaP StrontiumTitanate Kevlar Singapore lithography amplitude_modulation strontiu_titanate LiIonBattery hard_disk_media CompactDisk Moire Polydimethylsiloxane HDD PVA Regensburg Conductive AFM SiliconCrystal BCZT Aggregated_molecules suspended_graphene
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Star of Graphene
Scanning Conditions
- System : NX20
- Scan Mode: Non-contact
- Scan Rate : 0.6 Hz
- Scan Size : 2.5μm×2.5μm
- Pixel Size : 256×256
- Cantilever : Multi75-G (k=3N/m, f=75kHz)