CrystalGrowing GaN KPFM TransitionMetal HafniumDioxide piezoelectric force microscopy VerticalPFM Platinum BlockCopolymer atomic_steps dielectric_trench small_scan MagneticPhase FrictionalForceMicroscopy CeNSE_IISc DOE Moire GranadaUniv Pinpoint Ferrite BCZT Photovoltaics Spain Worcester_Polytechnic_Institute Lateral_Force_Microscopy oxide_layer phase_change Materials SoftSample Barium_titanate Chloroform LiNbO3 Polyvinylidene_fluoride PinpointNanomechanicalMode Copolymer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Nanostructures on polymer
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz
- Scan Size : 5μm×5μm
- Pixel Size : 256×256
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)