2d_materials PiezoelectricForceMicroscopy ShenYang Wonseok HACrystal sputter LateralForce Mapping STO ElectroChemical lift_mode biocompatible C_AFM Edwin MultiferroicMaterials fe_nd_b Au111 high_resolution non_contact Bismuth INSP UnivOfMaryland Titanate Hexatriacontane Polystyrene Lift #Materials TCS Hexylthiophene Semiconductor self-assembly CuSubstrate Polyimide medical self-assembled_monolayer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Copper Foil
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.5Hz
- Pixel: 512512