Mobile ElectroChemical Wonseok organic_polymer HighResolution HBN Gallium_Arsenide CuFoil PVAC BoronNitride Ceramics TemperatureControl molecular_self_assembly Self-assembledMonolayer Zagreb 2-vinylpyridine OpticalWaveguides Sidewall Modulus VerticalPFM KevlarFiber temperature controller AFM AtomicLayer SRAM epitaxy STM Wafer ReflexLens single_layer Annealed frequency_modulation blended polymers MfmAmplitude Ptfe CVD
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ITO glass
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm, 1μm×1μm
- Scan Rate: 0.4Hz, 1Hz
- Pixel: 512×512, 512×512