PinpointPFM Composite Hexatriacontane fluoroaalkane GaAs OpticalWaveguide Current SICM temperature controller AFM layers PolymerPatterns Blend mono_layer semifluorinated_alkane LateralForceMicroscopy StainlessSteel SSRM doped 2d_materials Graphite ferromagnetic GlassTemp cannabinoid SiWafer nanomechanical food Carbon PolyvinylideneFluoride Phenanthrene CHRYSALIS_INC PetruPoni heterojunctions HydroGel SFAs Display
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Phthalocyanine praseodymium
Scanning Conditions
- System: NX10
- Scan Mode: EFM
- Cantilever: PPP-EFM (k=2.8 N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel: 1024×256