2d_materials AM-KPFM Copolymer NUS Worcester_Polytechnic_Institute Thermal lithography PrCurve MagneticPhase LiquidCrystal AAO Austenite TungstenDeposition polyvinyl acetate MfmPhase VinylAlcohol kelvin probe force microscopy InLiquid Ceramics Deposition plastics DataStorage temp Writing BaTiO3 Biofilm MechanicalProperty BariumTitanate Sidewall CP-AFM DentalProsthesis cooling #EC TungstenThinFilmDeposition Chloroform
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Graphene on hBN
Scanning Conditions
- System : FX40
- Sample bias: 1 V
- Scan Mode: C-AFM
- Scan Rate : 25 Hz for 25 nm2, 10 Hz for 50 nm2
- Scan Size : 25nm2×25nm2
- Pixel Size : 128×128 for 25 nm2, 256×256 for nm2
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)